Skip to content

Copper Roofing & Cladding, Sydney

Copper changes colour more than any other metal we fold. It is bright salmon at install, brown within months and green over decades.

How it weathers

NewYear 50

Copper cladding and roofing by Roofing Group

Copper at a glance.

100+ years

Typical service life

Patina
Brown in months, green over 10 to 30 years
Maintenance
None required for the metal
Runoff
Stains and attacks zinc, aluminium and galvanised steel

How copper ages

New

Mill finish with a bright salmon lustre.

  1. NewMill finish with a bright salmon lustre.
  2. Year 1Oxidises to a warm, even brown.
  3. Year 5Deepens to chocolate brown.
  4. Year 10Near black; first green near the coast.
  5. Year 25Verdigris forms, faster in salt air.
  6. Year 50Full green patina protects the metal.

The copper timeline

New copper oxidises to warm brown within months, then darkens to chocolate and near black. Green verdigris follows, first on the most exposed faces. On the coast salt speeds this up; inland it can take several decades.

Pre-patinated and pre-oxidised sheets give a chosen colour from day one, for designs that cannot wait for the weather.

Where the water goes

Copper runoff stains masonry and paving green and corrodes zinc, aluminium and galvanised steel below it. We plan gutters, drips and material sequences so copper water never lands on another metal.

Folding copper

Copper is soft and forms cleanly, so it suits curves, shingles and detailed flashings. We fold standing seam, shingles, flat lock and interlocking panels in copper in our Sydney workshop.

Aurubis Nordic Copper

Copper finishes

15 finishes. Architectural copper from Aurubis, Europe’s largest copper producer and recycler. Select a swatch to see it larger.

Natural and oxidised

Mill finish copper that weathers on site, or factory-oxidised for an even brown from day one.

  • Nordic StandardBright mill finish
  • Nordic Brown LightPre-oxidised, light brown
  • Nordic BrownPre-oxidised, dark brown

Pre-patinated green

Factory green patina. Living versions leave some brown showing through, like natural weathering.

  • Nordic Green TraditionalFull green patina
  • Nordic Green Living 1Green patina, varied
  • Nordic Green Living 2Green patina, more varied

Pre-patinated blue

Blue and turquoise patinas for coastal and contemporary designs.

  • Nordic Blue TraditionalFull blue patina
  • Nordic Blue Living 1Blue patina, varied
  • Nordic Blue Living 2Blue patina, more varied
  • Nordic Blue Living 3Blue patina, most varied
  • Nordic TurquoiseTurquoise patina

Copper alloys

Golden and bronze tones for features, screens and facades.

  • Nordic BronzeCopper-tin alloy
  • Nordic BrassCopper-zinc alloy, golden yellow
  • Nordic Brass WeatheredPre-weathered brass
  • Nordic RoyalCopper, aluminium and zinc alloy, golden

Swatch images are published by the manufacturers. Screens vary, so ask us for physical samples before you specify.

Questions

9 answered

Copper questions

The questions estimators and drafters answer most often. If yours is not here, send the drawings and we will answer it against your project.

Ask about your project
How long does copper take to turn green in Sydney?

Near the coast, verdigris can start forming within about 8 to 15 years. Inland and on sheltered faces it can take 20 to 30 years or longer.

Can copper be used next to zinc?

Only if copper water never runs onto the zinc. Copper upstream of zinc will corrode it, so we detail the drainage sequence to prevent it.

Can we have the green finish straight away?

Yes. Pre-patinated sheet arrives green and pre-oxidised sheet arrives brown, so the elevation reads as intended on handover instead of in twenty years.

What thickness of copper do you fold?

0.6 mm for shingles and flat lock, 0.7 mm for standing seam and interlocking panels, and 1.5 mm for cassette trays.

Will copper stain the wall or paving below it?

Yes, unless the water is caught. Runoff carries copper salts that stain masonry, render and paving green. We plan the gutters, drips and material sequence so that water is collected rather than shed down the building.

What fixings and flashings go with copper?

Copper or stainless steel. Galvanised steel and aluminium corrode in contact with copper, so they do not appear anywhere in the assembly.

Is copper combustible?

No. Solid copper is non-combustible and classified A1 for reaction to fire. The whole wall assembly still has to be assessed, which we do per project.

Does copper need any maintenance?

None for the metal. It is doing the only thing it needs to do, which is weather. Gutters and outlets need the same clearing as any roof.

Why does copper cost more than zinc or aluminium?

The metal itself is dearer by weight, and copper tends to be specified on detailed work where there is more labour in the folding and the flashings. Against a 100 year service life it is usually the cheapest metal per year on the building.

Next metalAluminiumAluminium is light, does not rust and comes in almost any colour. It suits coastal facades and designs that need a consistent finish for decades.
All metals

Start your next project.

Send drawings or a brief. Concept sketches are enough to get a useful answer.

  1. You send drawings or a brief

    A plan, a section and an elevation are enough.

  2. 1business day

    An estimator replies

    Named contact, not a queue.

  3. 7days

    Tender returned

    Priced by system, metal and area.