Skip to content

Specification | | 7 min read

Zinc roofing and cladding: ventilation, substrates and underside corrosion

Ventilation gaps, substrates, membranes and fixings for zinc roofing and cladding, and how to detail the assembly to prevent underside corrosion.

Dark zinc standing seam wall cladding against a clear sky at Botanica, Ryde

Zinc protects itself with a patina that forms on the weather face. That patina needs air, carbon dioxide and regular drying. The back of a zinc sheet gets none of these unless the wall or roof provides them. If moisture sits against the underside of zinc without drying, the metal can corrode from behind, with nothing visible from outside until the damage is advanced.

The details below keep the underside dry on flat lock panels, shingles, standing seam and interlocking panels in zinc. Confirm the final assembly with the manufacturer’s current technical literature for the specific product.

Why zinc needs ventilation behind it

Warm, moist air from inside a building moves outward through the wall or roof. When it meets the cold back of a zinc sheet at night, it condenses. Rain or dew that gets behind the cladding at laps and junctions adds more water.

On the weather face, zinc forms a stable zinc carbonate patina through repeated wetting and drying in open air. On a sealed, damp underside, zinc hydroxide can form instead, often seen as white deposits. This underside corrosion thins the sheet over time and can leave it failing well short of its expected service life.

A continuous air gap behind the substrate lets that moisture dry out. Air enters at the base or eave, rises through the cavity and exits at the head or ridge.

Ventilated and unventilated assemblies

A ventilated assembly has a continuous air cavity between the substrate and the structure or insulation behind. It is the standard approach for zinc in Australia and suits most roofs and walls.

Some manufacturers offer unventilated or warm roof assemblies. These generally rely on a vapour control layer on the warm side, a specific separation or structured membrane under the zinc, and in some cases a factory applied coating on the underside of the zinc. Performance depends on every layer being installed as tested. Use a unventilated assembly only where the manufacturer’s current literature supports it for that product and application.

Feature Ventilated assembly Unventilated assembly
Air cavity Continuous, open at bottom and top None behind substrate
Moisture control Cavity airflow dries the substrate and zinc Vapour control layer and separation membrane
Typical use Most zinc roofs and walls Specific systems where the manufacturer supports it
Risk if detailed poorly Blocked vents reduce drying Trapped moisture with no escape path
Guidance Standard practice Confirm with manufacturer before specifying

Ventilation gaps

For flat lock panels and shingles in zinc, Roofing Group allows a continuous ventilation gap under the substrate of 20 mm on walls and 40 mm on roofs. The 40 mm roof gap applies to zinc only. Other metals and systems have their own requirements.

The gap must be continuous from inlet to outlet. Horizontal battens, noggings and blocking can cut off airflow, so use vertical battens or counter battens on walls, and keep eave and ridge vents clear. Insect mesh at inlets and outlets should have enough open area to keep air moving. For standing seam and interlocking panels, confirm cavity depth with the manufacturer for the specific assembly.

Substrates

Flat lock and shingle systems need a continuous, flat substrate. Construction grade plywood gives a flat, stable base. Timber boarding, laid with small gaps between boards, allows some airflow and drying from below.

Some timber preservatives can react with zinc, so check the plywood grade and any treatment on either substrate with the zinc manufacturer.

For interlocking panels, the panels fix to top hats (usually 1.15 mm galvanised) at max 600 mm centres, and the top hats create the cavity. A breathable vapour permeable membrane behind the top hats is recommended.

Membranes

On flat lock and shingle walls and roofs, Roofing Group wraps the substrate in a waterproofing membrane. The membrane sheds any water that passes the zinc and protects the substrate during construction.

Membrane choice depends on the assembly. A breathable vapour permeable membrane lets moisture escape outward while resisting liquid water. Some manufacturers specify a structured separation membrane directly under zinc to keep an air layer against the underside. Confirm the membrane type with the zinc manufacturer.

Incompatible materials

Zinc reacts with several common building materials. Keep them apart, and keep their runoff away.

Material Risk to zinc What to do
Western red cedar, oak and other acidic timbers Acidic runoff and contact corrode zinc Keep off the zinc and direct runoff clear
Copper Copper runoff and contact cause rapid corrosion Never drain copper onto zinc; isolate contact
Fresh cement, mortar and concrete Alkaline contact attacks zinc Separate with a membrane; keep mortar splashes off
Bitumen Runoff from bitumen products can attack zinc Avoid bitumen upslope of zinc and in direct contact
Carbon steel fixings and swarf Rust staining and galvanic corrosion Use stainless fixings; remove swarf daily

The same applies to materials upslope. A cedar clad upper storey or a copper flashing above a zinc wall can damage the zinc with every rain.

Fixings and clips

Use stainless steel clips and fixings with zinc. Stainless resists corrosion and, unlike carbon steel, does not leave rust stains on the zinc. Concealed stainless clips let standing seam and flat lock panels move with temperature.

For flat lock and shingle systems, clips sit at about 300 mm centres for residential work. Final spacing is set by the wind load for the site, the building height and the zone of the roof or wall.

Typical ventilated assembly, outside to inside

A ventilated zinc flat lock wall generally builds up as follows:

  1. Zinc flat lock panels or shingles.
  2. Concealed stainless steel clips at about 300 mm centres (to wind load).
  3. Waterproofing membrane wrapped over the substrate.
  4. Construction grade plywood or timber boarding substrate.
  5. Continuous ventilation cavity: 20 mm on walls, 40 mm on roofs.
  6. Vertical battens or counter battens forming the cavity.
  7. Breathable vapour permeable membrane.
  8. Insulation within the frame.
  9. Structural frame.
  10. Vapour control layer where the design requires it.
  11. Internal lining.

Layers 7, 8 and 10 depend on the building’s thermal and condensation design. Check them against the NCC and the project’s condensation assessment.

Checklist

  • Continuous ventilation gap of 20 mm (walls) or 40 mm (roofs, zinc only) under flat lock and shingle substrates.
  • Clear inlet and outlet at the bottom and top of every cavity.
  • Construction grade plywood or timber boarding substrate, treatment checked with the manufacturer.
  • Substrate wrapped in waterproofing membrane.
  • Stainless steel clips and fixings, spaced to wind load.
  • No acidic timber, copper, fresh cement or bitumen in contact with or draining onto zinc.
  • Unventilated assemblies only where the manufacturer supports them.

Next step

Mark cavity depths, vent locations and adjacent materials on your sections and send drawings for a shop drawing review. Our drafting team will return marked up assemblies before fabrication. See zinc, flat lock panels, shingles and standing seam, and download manufacturer literature from our downloads page.

Start your next project.

Send drawings or a brief. Concept sketches are enough to get a useful answer.

  1. You send drawings or a brief

    A plan, a section and an elevation are enough.

  2. 1business day

    An estimator replies

    Named contact, not a queue.

  3. 7days

    Tender returned

    Priced by system, metal and area.