A zinc gutter under a copper roof will fail. Not in twenty years, in three or four. It is the most common avoidable failure in architectural metalwork, and it is always a detailing decision rather than a material one.
What is actually happening
Put two different metals in contact with moisture between them and you have made a battery. One metal gives up electrons to the other and corrodes faster than it would alone. The less noble metal loses.
The order runs roughly: copper is the most noble, then stainless steel, then lead, then steel, then aluminium, then zinc. The further apart two metals sit on that list, the worse the reaction when they touch.
Three things have to be present for it to happen: two dissimilar metals, an electrical path between them, and an electrolyte, which on a roof means water. Remove any one and the reaction stops.
The two ways it happens
Direct contact. A copper flashing screwed to a zinc panel. A steel bracket bolted through aluminium. Metal on metal, with rain in the joint.
Runoff. This is the one that catches people. Water running off copper carries copper ions with it. Where that water lands on zinc, aluminium or Colorbond, it deposits those ions and the reaction starts, even though the two metals never touch.
Runoff is why a copper roof cannot drain into a zinc gutter, and why a copper feature panel above a Colorbond wall will stain and then corrode it. Water only goes one way, which is the saving grace: the metal below is at risk, the metal above is not.
What works and what does not
| Below | Copper above | Zinc above | Aluminium above | Steel above |
|---|---|---|---|---|
| Copper | Yes | Yes | Yes | Yes |
| Zinc | No | Yes | Yes | Check |
| Aluminium | No | Yes | Yes | Check |
| Colorbond | No | Yes | Yes | Yes |
| Stainless | Yes | Yes | Yes | Yes |
Copper sheds onto nothing except copper and stainless. Zinc and aluminium are close enough on the scale to sit together. Stainless steel is noble enough to be safe below anything and inert enough to be safe above most things, which is why clips and fixings are stainless across almost every system we fold.
Fixings are where it goes wrong
The panel gets specified carefully and the fastener gets left to site. Then a galvanised screw ends up through an aluminium panel, and the screw head is the anode in a joint that stays wet.
Two rules cover most of it:
Match the fixing to the panel, or go stainless. Our clips are stainless, which is compatible with everything, so the fixing is never the weak point in the joint.
Watch the small parts. Rivets, screws, washers, brackets, downpipe straps and gutter brackets are where dissimilar metals sneak in, because they are chosen by whoever is standing on the roof.
When you have to mix them
Sometimes the design wants copper above zinc. It can be done, but the detail has to carry it:
Break the contact. An inert separating layer, a butyl tape, a polymer washer or a membrane strip, stops the electrical path where two metals meet.
Break the drainage. Take the runoff from the upper metal into its own gutter or downpipe, so it never crosses the lower metal. On a facade that usually means a separate drainage line behind the junction rather than a visible gutter.
Use stainless as the buffer. A stainless flashing between copper and zinc works where a direct junction will not.
Change what is below. Often the cheapest answer. A stainless or copper gutter under a copper roof costs less than replacing a zinc one twice.
Sydney makes it worse
Salt air is an electrolyte. On a coastal site the water on the roof conducts better, so a galvanic pair that would be slow inland runs fast here.
That interacts with the corrosion zone question: a detail that is marginal in a suburban street is not marginal in Maroubra. If a project is within a few kilometres of the surf, we would treat any dissimilar metal junction as something to design out rather than manage.
What we check on a drawing set
When shop drawings come through our drafting team, these are the junctions that get looked at first:
- What the roof discharges into, and what that gutter is made of
- What the downpipes, brackets and straps are
- Every flashing where two different metals meet, including the ones drawn by someone else
- Fixings, rivets and washers, by material not just by size
- Any handrail, balustrade, plant platform or solar frame sitting on the roof
That last one is worth naming. A galvanised solar frame bolted through a zinc roof is a problem that arrives two years after handover, from a trade who never saw the roof specification.
If you have a junction you are unsure about, send the detail. We will tell you whether it stands up, and what to change if it does not. See zinc, copper and aluminium for how each metal behaves on its own, and corrosion zones in NSW for what the site does to all of it.